IEC61395 Creep Test Machine of Overhead Conductor
WLW-300 Computerized Horizontal Tensile Testing Machine
(লোড ক্ষমতা: 300kN, Creep Test)
1. Function:
The testing machine is mainly used to do creep test of overhead conductors, it also can be used for stress-strain test of overhead conductors. The testing machine adopts hydraulic cylinder to load, load cell to measure, computer to print and computer to display test data and other advanced technology.
2. Main Technical Specification
2.1 সর্বোচ্চ. পরীক্ষার শক্তি: 300KN
2.2 Rang of test force: 8kN-1000kN
2.3 পরীক্ষণ বলের যথার্থতা: better than ±1% of indicating value
2.4 Resolution of testing force: 1/100000
2.5 Testing space (not include piston stroke): 400-13000মিমি (500mm for interval)
2.6 Plug way: manual plug
2.7 Oil-cylinder piston stroke: 1500মিমি
2.8 Displacement measuring range: 1500মিমি
2.9 Resolution of displacement measuring: 0.01মিমি
2.10 Crossbeam quick tensile speed: not lower than 100mm/min
2.11 Load testing speed: 0-70মিমি/মিনিট
2.12 Height of work bench: 450মিমি
2.13 Testing force measuring way: load sensor 300kN
2.14 Control test method: computer auto control all the testing process, the testing force and testing
curve displayed on the PC, it auto process the testing date according to relative testing standard.
2.15 Clamp methods of specimen: hydraulic clamp, for connection part is supplied by the buyer.
2.16 Multiple testing curves displayed: force- displacement, force-time, force- deformation, stress-
strain, time- displacement, ইত্যাদি.
2.17 Control cabinet and mainframe is separated, it also has safety protection shield.
2.18 সামগ্রিক মাত্রা (L x W x H): 21000x1900x1455mm (for reference)
2.19 ওজন: 8000 kgs (for reference)
2.20 Power: 3 দশাটি, 4 wires, 380V±10%, 50হার্টজ